| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
| 物理性能 | 密度 | ASTM D-792 | 0.912 | g/cm3 | |
| 熔體流動速率 | 190℃/2.16 kg | ASTM D-1238 | 3.3 | g/10min | |
| 厚度 | 25 | microns | |||
| 機(jī)械性能 | 拉伸屈服強(qiáng)度 | MD | ASTM D-882 | 6.9 | MPa |
| 拉伸屈服強(qiáng)度 | TD | ASTM D-882 | 6.2 | MPa | |
| 斷裂伸長率 | MD | ASTM D-882 | 580 | % | |
| 斷裂伸長率 | TD | ASTM D-882 | 780 | % | |
| 埃爾曼多夫撕裂強(qiáng)度 | MD | ASTM D-1922 | 400 | g | |
| 埃爾曼多夫撕裂強(qiáng)度 | TD | ASTM D-1922 | 590 | g | |
| 埃爾曼多夫撕裂強(qiáng)度 | MD | ASTM D-1922 | 16 | g/micron | |
| 埃爾曼多夫撕裂強(qiáng)度 | TD | ASTM D-1922 | 23.6 | g/micron | |
| 落錘沖擊 | |
ASTM D-1709 | 18.4 | g | |
| 拉伸斷裂強(qiáng)度 | MD | ASTM D-882 | 56.5 | MPa | |
| 拉伸斷裂強(qiáng)度 | TD | ASTM D-882 | 36.5 | MPa | |
| 熱性能 | 熔融溫度 | 274 | ℃ | ||
| 維卡軟化點(diǎn) | 90 | ℃ | |||
| 光學(xué)性能 | 霧度 | 0.8 | % | ||
| 光澤度 | 95 | % | |||