| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
| 物理性能 | 密度 | ASTM D-1505 | 0.833 | g/cm3 | |
| 熔點(diǎn) | MCI方法 | 240 | ℃ | ||
| 熔融指數(shù) | 260℃,5kg | ASTM D-1238 | 180 | g/10min | |
| 機(jī)械性能 | 凹口Charpy耐沖擊強(qiáng)度 | ASTM D-256 | --- | kgcm/cm2 | |
| Rockwell硬度 | ASTM D-785 | R80 | |||
| 無(wú)凹口lzod耐沖擊強(qiáng)度 | ASTM D-256 | --- | kgcm/cm2 | ||
| 曲折模數(shù) | ASTM D-790 | 13,000 | kg/cm2 | ||
| 斷裂伸長(zhǎng)率 | ASTM D-638 | 20 | % | ||
| Olsen剛性 | ASTM D-747 | 8,800 | kg/cm2 | ||
| 抗張強(qiáng)度 | ASTM D-638 | 175 | kg/cm2 | ||
| 抗張屈服強(qiáng)度 | ASTM D-638 | 230 | kg/cm2 | ||
| 曲折強(qiáng)度 | ASTM D-790 | 360 | kg/cm2 | ||
| 電氣性能 | 介電消散因子 | 23℃,1MHz | ASTM D-150 | 0.0012 | |
| 吸水率 | ASTM D-570 | 0.01 | % | ||
| 體積電阻系數(shù) | ASTM D-257 | >1016 | Ωcm | ||
| 介電強(qiáng)度 | ASTM D-149 | 65 | KV/mm | ||
| 介電常數(shù) | 100~1MHz | ASTM D-150 | 2.12 | ||
| 熱性能 | 模收縮率(機(jī)械/垂直方向) | MCI方法 | --- | % | |
| 燃燒速率 | ASTM D-635 | 2.54 | cm/min | ||
| 線膨脹系數(shù) | ASTM D-696 | 1.17*10-4 | 1/℃ | ||
| 比熱 | ASTM C-351 | 0.47 | cal/g℃ | ||
| 熱傳導(dǎo)系數(shù) | ASTM BS-847A | 4*10-4 | calcm/seccm2℃ | ||
| 熱變形溫度 | 4.6kg/cm2 | ASTM D-648 | --- | ℃ | |
| Vicat軟化點(diǎn) | ASTM D-1525 | 173 | ℃ | ||
| 其它性能 | 模糊度 | ASTM D-1746 | --- | % | |
| 透光率 | ASTM D-1746 | --- | % | ||
| 折射率 | ASTM D-542 | --- | nd | ||