| 斷裂伸長(zhǎng)率 | 530% | 密度 | 1.16g/cm3 | 熔體流動(dòng)速率 | 3g/10min |
| 吸水率 | 0.4% | 硬度 | 50 |
|
|
產(chǎn)品簡(jiǎn)述
| 斷裂伸長(zhǎng)率 | 530% | 密度 | 1.16g/cm3 | 熔體流動(dòng)速率 | 3g/10min |
| 吸水率 | 0.4% | 硬度 | 50 |
詳細(xì)數(shù)據(jù)
訂購(gòu)指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 24小時(shí)吸水率 | ASTM D-570 | 0.4 | % | ||
| 物理性能 | 比重 | ASTM D-792 | 1.16 | |||
| 熔體流動(dòng)速率 | ASTM D-1238 | 3.0 | g/10min | |||
| 泰伯磨耗量 | H 18輪 | ASTM D-1044 | 186 | mg/1000rev | ||
| 泰伯磨耗量 | CS-17輪 | ASTM D-1044 | 38 | mg/1000rev | ||
| 機(jī)械性能 | 揉曲模量 | 23℃ | ASTM D-790 | 124 | MPa | |
| 埃佐沖擊強(qiáng)度 | 23℃ | ASTM D-256 | 不破裂 | J/m | ||
| 初耐撕裂性能 | ASTM D-1004 | 145 | kn/m | |||
| 硬度計(jì)硬度 | ASTM D-2240 | 50 | ||||
| 拉伸力 | 5%伸長(zhǎng) | ASTM D-638 | 5.5 | MPa | ||
| 10%伸長(zhǎng) | ASTM D-638 | 8.3 | MPa | |||
| 斷裂伸長(zhǎng) | ASTM D-638 | 530 | % | |||
| 斷裂拉伸力 | ASTM D-638 | 36 | MPa | |||
| 熱性能 | 熱畸變溫度 | @0.18Mpa | ASTM D-648 | 44 | ℃ | |
| 維卡軟化點(diǎn) | ASTM D-1525 | 155 | ℃ | |||
| 熔點(diǎn) | ASTM D-3418 | 196 | ℃ | |||
| 熱畸變溫度 | @0.5Mpa | ASTM D-648 | 62 | ℃ | ||
| 其它性能 | 耐揉曲切口增長(zhǎng)性能 | ASTM D-1052 | 6×105 | |||