| 拉伸強度 | 55.8MPa | 密度 | 1.4g/cm3 | 熔體流動速率 | 9g/10min |
| 吸水率 | 0.22% | 規(guī)格級別 | 耐磨 | 成型收縮率 | 2% |
| 特性級別 | 耐磨,耐高溫 |
|
|
產(chǎn)品簡述
| 拉伸強度 | 55.8MPa | 密度 | 1.4g/cm3 | 熔體流動速率 | 9g/10min |
| 吸水率 | 0.22% | 規(guī)格級別 | 耐磨 | 成型收縮率 | 2% |
| 特性級別 | 耐磨,耐高溫 |
詳細數(shù)據(jù)
訂購指南
| 性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 物理性能 | 比重 | ASTM D792 | 1.4 | |||
| 吸水率 | ASTM D570 | 0.22 | % | |||
| 成型收縮率 | ASTM D955 | 2.0 | % | |||
| 機械性能 | 拉伸強度 | ASTM D638 | 570 | kg/cm2 | ||
| 拉伸率 | ASTM D638 | 70 | % | |||
| 彎曲強度 | ASTM D790 | 750 | kg/cm2 | |||
| 彎曲彈性率 | ASTM D790 | 25000 | kg/cm2 | |||
| Izod缺口沖擊強度 | ASTM D256 | 6.0 | Kg/cm.cm | |||
| 洛氏硬度 | ASTM D785 | 80 | M | |||
| 摩擦系數(shù) | ASTM D1894 | 0.11 | ||||
| 電氣性能 | 表面電阻率 | ASTM D257 | 1×1016 | Ω.cm | ||
| 體積電阻率 | ASTM D257 | 1×1014 | Ω | |||
| 熱性能 | 熔融指數(shù) | ASTM D1238 | 9.0 | g/10min | ||
| 熔點 | ASTM D1525 | 166 | ℃ | |||
| 熱變形溫度 | - | 0.45MPa | ASTM D648 | 160 | ℃ | |
| - | 1.82MPa | ASTM D648 | 110 | ℃ | ||
| 阻燃性 | UL94 | HB | ||||
| 線膨脹系數(shù) | ASTM D696 | 11-13 | ||||