| 斷裂伸長率 | 550% | 拉伸強(qiáng)度 | 17MPa | 密度 | 0.922g/cm3 |
| 熔體流動速率 | 2g/10min | 維卡軟化點(diǎn) | 103℃ | 用途級別 | 薄膜級 |
| 規(guī)格級別 | 薄膜 | 加工級別 | 吹塑級 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 550% | 拉伸強(qiáng)度 | 17MPa | 密度 | 0.922g/cm3 |
| 熔體流動速率 | 2g/10min | 維卡軟化點(diǎn) | 103℃ | 用途級別 | 薄膜級 |
| 規(guī)格級別 | 薄膜 | 加工級別 | 吹塑級 |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 密度 | ASTM D-1505 | 0.922 | g/cm3 | ||
| 機(jī)械性能 | 斷裂點(diǎn)抗張強(qiáng)度 | MD | ASTM D-882 | 250 | kg/cm2 | |
| TD | ASTM D-882 | 180 | kg/cm2 | |||
| 抗沖擊強(qiáng)度 | ASTM D-1709 | 150 | g/F50 | |||
| 降伏點(diǎn)抗張強(qiáng)度 | MD | ASTM D-882 | 115 | kg/cm2 | ||
| TD | ASTM D-882 | 100 | kg/cm2 | |||
| 熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 103 | ℃ | ||
| 其它性能 | 伸長率 | ASTM D-882 | 550 | % | ||
| 收縮率 | ASTM D-995 | 2 | % | |||
| 熔融指數(shù) | ASTM D-1238 | 2.0 | g/10min | |||
| 伸長率 | ASTM D-882 | 450 | % | |||
| 低溫脆裂溫度 | ASTM D-746 | <-76 | ℃ | |||
| 熔點(diǎn) | ASTM D-2117 | 124 | ℃ | |||