| 規(guī)格級(jí)別 | 注塑 | 加工級(jí)別 | 注塑級(jí) |
|
|
產(chǎn)品簡(jiǎn)述
| 規(guī)格級(jí)別 | 注塑 | 加工級(jí)別 | 注塑級(jí) |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 密度 | ASTM D-1505 | 0.924 | g/cm3 | ||
| 熔體流動(dòng)速率 | ASTM D-1238 | 20.0 | g/10min | |||
| 機(jī)械性能 | 斷裂伸長(zhǎng)率 | MD | ASTM D-882 | 600 | % | |
| TD | ASTM D-882 | - | % | |||
| 斷裂拉伸強(qiáng)度 | MD | ASTM D-882 | 120 | Kg/cm2 | ||
| TD | ASTM D-882 | - | Kg/cm2 | |||
| 屈服拉伸強(qiáng)度 | MD | ASTM D-882 | 150 | Kg/cm2 | ||
| TD | ASTM D-882 | - | Kg/cm2 | |||
| 抗張模數(shù) | MD | ASTM D-882 | 2500 | Kg/cm2 | ||
| TD | ASTM D-882 | - | Kg/cm2 | |||
| 邵氏硬度 | ASTM D-2240 | 52 | ||||
| 熱性能 | 低溫脆化溫度 | ASTM D-746 | <-70 | ℃ | ||
| 維卡軟化點(diǎn) | ASTM D-1525 | 90 | ℃ | |||