| 斷裂伸長率 | 800% | 拉伸強度 | 34MPa | 密度 | 0.918g/cm3 |
| 熔體流動速率 | 2.1g/10min | 維卡軟化點 | 98℃ | 用途級別 | 薄膜級,纖維 |
| 規(guī)格級別 | 薄膜 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 800% | 拉伸強度 | 34MPa | 密度 | 0.918g/cm3 |
| 熔體流動速率 | 2.1g/10min | 維卡軟化點 | 98℃ | 用途級別 | 薄膜級,纖維 |
| 規(guī)格級別 | 薄膜 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 熔體流動速率 | ASTM D-1238 | 2.1 | g/10min | ||
| 密度 | ASTM D-1505 | 0.918 | g/cm3 | |||
| 物理性能 | 薄膜厚度 | 25 | µm | |||
| 機械性能 | 拉伸斷裂強度 | MD | ASTM D-882 | 400 | Kg/cm2 | |
| TD | ASTM D-882 | 350 | Kg/cm2 | |||
| 撕裂強度 | MD | ASTM D-1004 | 120 | Kg/cm | ||
| TD | ASTM D-1004 | 110 | Kg/cm | |||
| 抗張模數(shù) | MD | ASTM D-882 | 2200 | Kg/cm2 | ||
| TD | ASTM D-882 | 3100 | Kg/cm2 | |||
| 拉伸屈服強度 | MD | ASTM D-882 | 140 | Kg/cm2 | ||
| TD | ASTM D-882 | 130 | Kg/cm2 | |||
| 尖頭沖擊強度 | ASTM D-1709 | 4.0 | g/μm | |||
| 斷裂伸長率 | MD | ASTM D-882 | 650 | % | ||
| TD | ASTM D-882 | 800 | % | |||
| 熱性能 | 維卡軟化點 | ASTM D-1525 | 98 | ℃ | ||
| 低溫脆化溫度 | ASTM D-746 | <-80 | ℃ | |||