| 斷裂伸長率 | 600% | 拉伸強度 | 14.5MPa | 密度 | 0.918g/cm3 |
| 熔體流動速率 | 0.25g/10min | 規(guī)格級別 | 吹塑 | 彎曲模量 | 234MPa |
| 加工級別 | 吹塑級,發(fā)泡級 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 600% | 拉伸強度 | 14.5MPa | 密度 | 0.918g/cm3 |
| 熔體流動速率 | 0.25g/10min | 規(guī)格級別 | 吹塑 | 彎曲模量 | 234MPa |
| 加工級別 | 吹塑級,發(fā)泡級 |
詳細數(shù)據(jù)
訂購指南
| 性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||||
| 基本性能 | 密度 | ASTM D-1505 | 0.918 | g/cm3 | ||||
| 熔體流動速率 | 190℃/2.16kg | ASTM D-1238 | 0.25 | g/10min | ||||
| 機械性能 | 環(huán)境應力開裂 | 0% Igepal, F0 | ASTM D-1693 | 168 | hr | |||
| 邵氏硬度 | Shore D | ASTM D-2240 | 50 | |||||
| 拉抻斷裂強度 | ASTM D-638 | 14.5 | MPa | |||||
| 拉伸斷裂伸長率 | ASTM D-638 | 600 | % | |||||
| 彎曲模量 | ASTM D-790 | 234 | MPa | |||||
| 薄膜厚度-Tested | 50.8 | um | ||||||
| 割線模量-1% Secant | 50.8um | ASTM D-882 |
|
MPa | ||||
| 拉抻屈服強度 | 50.8um | ASTM D-882 |
|
MPa | ||||
| 拉伸斷裂伸長率 | ASTM D-882 | ASTM D-882 |
|
% | ||||
| 落錘沖擊 | 50.8um | ASTM D-1709 | 220 | g | ||||
| 埃爾曼多夫撕裂強度 | 50.8um | ASTM D-1922 |
|
g | ||||
| 加工性能 | 熔體溫度 | 166-221 | ℃ | |||||
| 熱性能 | 脆化溫度 | ASTM D-746 | -76 | ℃ | ||||
| 維卡軟化點 | ASTM D-1525 | 90 | ℃ | |||||