| 斷裂伸長(zhǎng)率 | 420% | 拉伸強(qiáng)度 | 10MPa | 密度 | 0.918g/cm3 |
| 熔體流動(dòng)速率 | 6g/10min | 用途級(jí)別 | 薄膜級(jí) | 規(guī)格級(jí)別 | 薄膜 |
| 缺口沖擊強(qiáng)度 | 110 |
|
|
產(chǎn)品簡(jiǎn)述
| 斷裂伸長(zhǎng)率 | 420% | 拉伸強(qiáng)度 | 10MPa | 密度 | 0.918g/cm3 |
| 熔體流動(dòng)速率 | 6g/10min | 用途級(jí)別 | 薄膜級(jí) | 規(guī)格級(jí)別 | 薄膜 |
| 缺口沖擊強(qiáng)度 | 110 |
詳細(xì)數(shù)據(jù)
訂購(gòu)指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 密度 | 23°C | ASTM D-1505 | 0.918 | g/cm3 | |
| 熔體流動(dòng)速率 | ASTM D-1238 | 6.0 | g/10min | |||
| 機(jī)械性能 | 跌落沖擊強(qiáng)度 | ASTM D-1709 | 110 | g | ||
| 抗張強(qiáng)度 | ASTM D-638 | 110 | Kg/cm2 | |||
| 抗撕裂張度 | MD | ASTM D-1922 | 250 | g | ||
| TD | ASTM D-1922 | 300 | g | |||
| 屈服點(diǎn)張力 | ASTM D-638 | 90 | Kg/cm2 | |||
| 破裂點(diǎn)張力 | MD | ASTM D-882 | 180 | kg/cm2 | ||
| TD | ASTM D-882 | 160 | kg/cm2 | |||
| 斷裂伸長(zhǎng)率 | ASTM D-638 | 420 | % | |||
| 斷裂點(diǎn)伸張率 | MD | ASTM D-882 | 380 | % | ||
| TD | ASTM D-882 | 530 | % | |||
| 熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 88 | °C | ||
| 低溫脆化溫度 | ASTM D-746 | <-76 | °C | |||