| 斷裂伸長率 | 580% | 拉伸強(qiáng)度 | 14MPa | 密度 | 0.924g/cm3 |
| 熔體流動速率 | 0.8g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 吹塑 |
| 缺口沖擊強(qiáng)度 | 150 | 加工級別 | 擠出級,吹塑級 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 580% | 拉伸強(qiáng)度 | 14MPa | 密度 | 0.924g/cm3 |
| 熔體流動速率 | 0.8g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 吹塑 |
| 缺口沖擊強(qiáng)度 | 150 | 加工級別 | 擠出級,吹塑級 |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 熔體流動速率 | ASTM D-1238 | 0.8 | g/10min | ||
| 密度 | ASTM D-1505 | 0.924 | g/cm3 | |||
| 機(jī)械性能 | 破裂點(diǎn)張力 | MD | ASTM D-882 | 275 | kg/cm2 | |
| TD | ASTM D-882 | 235 | kg/cm2 | |||
| 抗撕裂張度 | MD | ASTM D-1922 | 280 | g | ||
| TD | ASTM D-1922 | 280 | g | |||
| 斷裂伸長率 | ASTM D-638 | 580 | % | |||
| 抗張強(qiáng)度 | ASTM D-638 | 150 | Kg/cm2 | |||
| 斷裂點(diǎn)伸張率 | MD | ASTM D-882 | 490 | % | ||
| TD | ASTM D-882 | 600 | % | |||
| 跌落沖擊強(qiáng)度 | ASTM D-1709 | 150 | g | |||
| 屈服點(diǎn)張力 | ASTM D-638 | 115 | Kg/cm2 | |||
| 熱性能 | 低溫脆化溫度 | ASTM D-746 | <-76 | °C | ||
| 維卡軟化點(diǎn) | ASTM D-1525 | 97 | °C | |||