| 斷裂伸長率 | 600% | 拉伸強(qiáng)度 | 14MPa | 密度 | 0.924g/cm3 |
| 熔體流動速率 | 2.1g/10min | 缺口沖擊強(qiáng)度 | 100 | 加工級別 | 注塑級 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 600% | 拉伸強(qiáng)度 | 14MPa | 密度 | 0.924g/cm3 |
| 熔體流動速率 | 2.1g/10min | 缺口沖擊強(qiáng)度 | 100 | 加工級別 | 注塑級 |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 密度 | ASTM D-1505 | 0.924 | g/cm3 | ||
| 熔體流動速率 | ASTM D-1238 | 2.1 | g/10min | |||
| 機(jī)械性能 | 拉力降伏強(qiáng)度 | ASTM D-638 | 100 | kg/cm2 | ||
| 拉力降伏強(qiáng)度 | MD | ASTM D-882B | 100 | kg/cm2 | ||
| TD | ASTM D-882B | 110 | kg/cm2 | |||
| 抗撕裂性 | MD | ASTM D-1922 | 70 | N/mm | ||
| TD | ASTM D-1922 | 50 | N/mm | |||
| 拉力斷裂伸長率 | MD | ASTM D-882B | 280 | % | ||
| TD | ASTM D-882B | 580 | % | |||
| 彎曲模量 | ASTM D-790 | 1800 | kg/cm2 | |||
| 拉力斷裂強(qiáng)度 | MD | ASTM D-882B | 230 | kg/cm2 | ||
| TD | ASTM D-882B | 180 | kg/cm2 | |||
| 1%伸長彈性系數(shù) | MD | ASTM D-882B | 2000 | kg/cm2 | ||
| TD | ASTM D-882B | 2300 | kg/cm2 | |||
| 拉力斷裂伸長率 | ASTM D-638 | 600 | % | |||
| 硬度 | ASTM D-2240 | 53 | Shore D | |||
| 拉力斷裂強(qiáng)度 | ASTM D-638 | 150 | kg/cm2 | |||
| 摩擦系數(shù) | ASTM D-1894 | >0.5 | ||||
| 落球行動強(qiáng)度 | ASTM D-1709 | 100 | g | |||
| 熱性能 | 軟化點(diǎn) | ASTM D-1525 | 96 | ℃ | ||
| 脆化溫度 | ASTM D-746 | <-70 | ℃ | |||
| 熔點(diǎn) | DSC | 113 | ℃ | |||
| 其它性能 | 光澤度 | 45℃ | ASTM D-2457 | 95 | % | |
| 濁度 | ASTM D-1003 | 6.5 | % | |||
| 建設(shè)薄膜厚度 | ASTM D-1003 | 25~80 | µ | |||