| 斷裂伸長率 | 550% | 拉伸強(qiáng)度 | 20MPa | 密度 | 0.922g/cm3 |
| 熔體流動速率 | 0.25g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
| 缺口沖擊強(qiáng)度 | 280 | 加工級別 | 注塑級 | 特性級別 | 增強(qiáng)級 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 550% | 拉伸強(qiáng)度 | 20MPa | 密度 | 0.922g/cm3 |
| 熔體流動速率 | 0.25g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
| 缺口沖擊強(qiáng)度 | 280 | 加工級別 | 注塑級 | 特性級別 | 增強(qiáng)級 |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 熔體流動速率 | ASTM D-1238 | 0.25 | g/10min | ||
| 密度 | ASTM D-1505 | 0.922 | g/cm3 | |||
| 機(jī)械性能 | 落球沖擊強(qiáng)度 | ASTM D-1709 | 280 | g | ||
| 抗撕裂性 | MD | ASTM D-1922 | 25 | N/mm | ||
| TD | ASTM D-1922 | 35 | N/mm | |||
| 斷裂點(diǎn)強(qiáng)度 | MD | ASTM D-882B | 230 | kg/cm2 | ||
| TD | ASTM D-882B | 210 | kg/cm2 | |||
| 斷裂點(diǎn)伸長率 | MD | ASTM D-882B | 350 | % | ||
| TD | ASTM D-882B | 550 | % | |||
| 降伏點(diǎn)強(qiáng)度 | MD | ASTM D-882B | 100 | kg/cm2 | ||
| TD | ASTM D-882B | 110 | kg/cm2 | |||
| 1%伸長彈性系數(shù) | MD | ASTM D-882B | 1650 | kg/cm2 | ||
| TD | ASTM D-882B | 1850 | kg/cm2 | |||
| 熱性能 | 脆化溫度 | ASTM D-746 | <-75 | ℃ | ||
| 軟化點(diǎn) | ASTM D-1525 | 96 | ℃ | |||
| 熔點(diǎn) | DSC | 113 | ℃ | |||
| 其它性能 | 薄膜厚度 | 60-250 | ц | |||
| 濁度 | ASTM D-1003 | 20 | % | |||
| 摩擦系數(shù) | ASTM D-1894 | >0.5 | ||||
| 光澤度 | 45℃ | ASTM D-2457 | 30 | % | ||