| 斷裂伸長率 | 750% | 拉伸強(qiáng)度 | 16MPa | 密度 | 0.922g/cm3 |
| 熔體流動(dòng)速率 | 0.3g/10min | 規(guī)格級別 | 薄膜級 | 缺口沖擊強(qiáng)度 | 130 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 750% | 拉伸強(qiáng)度 | 16MPa | 密度 | 0.922g/cm3 |
| 熔體流動(dòng)速率 | 0.3g/10min | 規(guī)格級別 | 薄膜級 | 缺口沖擊強(qiáng)度 | 130 |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 |
| 密度 | ASTM D-1505 | 0.922 | g/cm3 | |
| 斷裂拉伸強(qiáng)度(MD) | ASTM D-882 | 200 | kg/cm2 | |
| 斷裂拉伸強(qiáng)度(TD) | ASTM D-882 | 190 | kg/cm2 | |
| 延伸率(MD) | ASTM D-882 | 320 | % | |
| 延伸率(TD) | ASTM D-882 | 580 | % | |
| Dart Drop沖擊強(qiáng)度 | ASTM D-1709 | 130 | g | |
| 屈服拉伸強(qiáng)度 | 50mm/min | ASTM D-638 | 115 | kg/cm2 |
| Dart Drop沖擊強(qiáng)度 | ASTM D-1709 | 130 | g | |
| 斷裂拉伸強(qiáng)度 | 50mm/min | ASTM D-638 | 170 | kg/cm2 |
| 斷裂延伸率 | 50mm/min | ASTM D-638 | 750 | % |
| 維卡軟化點(diǎn) | 1kg | ASTM D-1525 | 92 | ℃ |
| 摩擦系數(shù) | ASTM D-1894 | 0.3 | ||
| 脆化溫度 | ASTM D-746 | ℃ | ||
| 熔融指數(shù) | 190℃,2.16kg | ASTM D-1238 | 0.3 | g/10min |
| 彎曲硬度 | ASTM D-747 | 2400 | kg/cm2 | |
| 熔點(diǎn) | ASTM SGC | 111 | ℃ |