| 斷裂伸長率 | 800% | 拉伸強(qiáng)度 | 17MPa | 密度 | 0.925g/cm3 |
| 熔體流動速率 | 1g/10min | 硬度 | 46 | 用途級別 | 薄膜級 |
| 規(guī)格級別 | 薄膜 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 800% | 拉伸強(qiáng)度 | 17MPa | 密度 | 0.925g/cm3 |
| 熔體流動速率 | 1g/10min | 硬度 | 46 | 用途級別 | 薄膜級 |
| 規(guī)格級別 | 薄膜 |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||||
| 基本性能 | 密度 | ASTM D-1505 | 0.925 | g/cm3 | ||||
| 熔體流動速率 | ASTM D-1238 | 1.0 | ||||||
| VA含量 | 5.0 | % | ||||||
| 機(jī)械性能 | 拉伸屈服 | ASTM D-638 | 9 | MPa | ||||
| 拉伸斷裂 | ASTM D-638 | 17 | MPa | |||||
| 極限伸長率 | ASTM D-638 | 800 | % | |||||
| 1%正割模量 | ASTM D-638 | 207 | MPa | |||||
| 邵氏硬度 | ASTM D-2240 | 46 | ||||||
| 落錘沖擊 | ASTM D-1709 | 200 | g | |||||
| 極限伸長率 | ASTM D-882 |
|
% | |||||
| 拉伸斷裂強(qiáng)度 | ASTM D-882 |
|
MPa | |||||
| 1%正割模量 | ASTM D-882 |
|
MPa | |||||
| 熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 87 | ℃ | ||||
| 其它性能 | 熔體溫度范圍 | ASTM D-1525 | 182-193 | ℃ | ||||
| 光學(xué)性能 | 霧度 | ASTM D-1003 | 5.0 | % | ||||
| 光澤度 | ASTM D-523 | 73 | ||||||