| 斷裂伸長率 | 650% | 拉伸強(qiáng)度 | 27MPa | 密度 | 0.929g/cm3 |
| 熔體流動速率 | 0.3g/10min | 維卡軟化點(diǎn) | 73℃ | 用途級別 | 薄膜級 |
| 規(guī)格級別 | 薄膜 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 650% | 拉伸強(qiáng)度 | 27MPa | 密度 | 0.929g/cm3 |
| 熔體流動速率 | 0.3g/10min | 維卡軟化點(diǎn) | 73℃ | 用途級別 | 薄膜級 |
| 規(guī)格級別 | 薄膜 |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||||
| 基本性能 | 比重 | ASTM D-1505 | 0.929 | g/cm3 | ||||
| 熔體質(zhì)量流動速率 | 190℃/2.16kg | ASTM D-1238 | 0.30 | g/10min | ||||
| VA含量 | 12 | wt% | ||||||
| 機(jī)械性能 | 耐環(huán)境應(yīng)力開裂性 | 100% lgepal F50 | ASTM D-1693 | >300 | Hr | |||
| 拉伸屈服強(qiáng)度 | ASTM D-638 | 6 | MPa | |||||
| 拉伸斷裂強(qiáng)度 | ASTM D-638 | 27 | MPa | |||||
| 斷裂伸長率 | ASTM D-638 | 650 | % | |||||
| 摩擦系數(shù) | ASTM D-1894 | >1.0 | ||||||
| 拉伸屈服強(qiáng)度 | 30.0µm | ASTM D-882 |
|
MPa | ||||
| 拉伸斷裂強(qiáng)度 | 30.0µm | ASTM D-882 |
|
MPa | ||||
| 斷裂伸長率 | 30.0µm | ASTM D-882 |
|
% | ||||
| 埃爾曼多夫撕裂強(qiáng)度 | 0.0300mm | ASTM D-1922 |
|
kN/m | ||||
| 熱性能 | 脆化溫度 | ASTM D-746 | <-50 | ℃ | ||||
| 維卡軟化溫度 | ASTM D-1525 | 73 | ℃ | |||||
| 熔化溫度 | ASTM D-3418 | 95 | ℃ | |||||
| 光學(xué)性能 | 光澤度 | 60° | ASTM D-2457 | 53 | ||||