| Typical Properties | ||
| Property | Typical Value, Units | |
| Form | Powder | |
| Acetyl Content | 1.3 wt % | |
| Propionyl Content | 48 wt % | |
| Hydroxyl Content | 1.7 wt % | |
| Melting Point | 188-210°C | |
| Acidity as Acetic Acid | 0.01 wt % | |
| Ash Content | 0.017 wt % | |
| Refractive Index | 1.475 n(25°C/D) | |
| Glass Transition Temperature (Tg) | 147°C | |
| Specific Gravity @ 20°C/25°C | 1.22 | |
| Wt/Vol @ 20°C | 1.22 kg/L (10.2 lb/gal) | |
| Tukon Hardness | 23 Knoops | |
| Viscosity a | 76.5 poise | |